A nickel-chromium-molybdenum-tungsten alloy, Alloy 22 offers outstanding corrosion resistance in highly aggressive environments across a wide range of industries.
Alloy 22, also known as Hastelloy® C-22 and Inconel® 22, is a high-performance corrosion-resistant alloy made from nickel, chromium, molybdenum, and tungsten.
It offers outstanding resistance to pitting, crevice corrosion, and stress corrosion cracking (SCC), even in highly aggressive chloride-rich and acidic environments. Engineered to perform in both oxidising and reducing conditions, Alloy 22 is trusted across chemical processing, marine, aerospace, and pollution control industries.
% | Ni | Cr | Mo | Fe | W | Co | C | Mn | Si | V | P | S |
---|---|---|---|---|---|---|---|---|---|---|---|---|
Min | Balance | 20 | 12.5 | 2 | 2.5 | - | - | - | - | - | - | - |
Max | - | 22.5 | 14.5 | 6 | 3.5 | 2.5 | 0.015 | 0.5 | 0.08 | 0.35 | 0.02 | 0.02 |
Mechanical & Physical Properties | -196⁰C | 20⁰C | 100⁰C | 200⁰C | 300⁰C | 400⁰C |
---|---|---|---|---|---|---|
Ultimate Tensile Strength for sheet ≤ 50 mm thick | 690-950 | |||||
Ultimate Tensile Strength for bar ≤ 90 mm thick | 690-951 | |||||
0.2% Yield Strength for sheet ≤ 50 mm thick | 310 | 270 | 225 | 195 | 175 | |
0.2% Yield Strength for bar ≤ 90 mm thick | 310 | 290 | 245 | 215 | 195 | |
Elongation, % for sheet ≤ 50 mm thick | 45 | |||||
Elongation, % for bar ≤ 90 mm thick | 45 | |||||
Charpy Impact V-notch men value / J | 96 | 120 | ||||
Thermal Conductivity | 10.1 | 11.1 | 13.4 | 15.5 | 17.5 | |
Modulus of Elasticity / 105MPA | 2.05 | 1.97 | 1.85 |
Media | Common Name | Temp. °F (°C) | Corrosion Rate (mpy) |
---|---|---|---|
99% C2H4O2 | Acetic Acid | Boiling | NIL |
10% FeCl3 | Ferric Chloride | Boiling | 1 |
88% CH2O2 | Formic Acid | Boiling | <1 |
1% HCl | Hydrochloric Acid | Boiling | 3 |
5% HCl | Hydrochloric Acid | 158 (70) | 19 |
10% HCl | Hydrochloric Acid | Boiling | 400 |
5% HCl + 42 g/l Fe2(SO4)3 | Mixed Acid | 150 (66) | 2 |
5% HCl + 2% HF | Mixed Acid | 158 (70) | 59 |
5% HF | Hydrofluoric Acid | 158 (70) | 14 |
85% H3PO4 | Phosphoric Acid | Boiling | 13 |
44% P2O5 | Phosphoric Oxide | 240 (116) | 21 |
38% P2O5 + 2000ppm Cl | Mixed Acid | 185 (85) | 1 |
38% P2O5 + 0.5% HF | Mixed Acid | 185 (85) | 7 |
10% HNO3 | Nitric Acid | Boiling | <1 |
65% HNO3 | Nitric Acid | Boiling | 134 |
5% HNO3 + 6% HF | Mixed Acid | 140 (60) | 67 |
5% HNO3 + 25% H2SO4 + 4% NaCl | Mixed Acid | Boiling | 12 |
5% HNO3 + 1% HCl | Mixed Acid | Boiling | <1 |
5% HNO3 + 2.5% HCl | Mixed Acid | Boiling | 2 |
8.8% HNO3 +15.8% HCl | Mixed Acid | 126 (52) | 4 |
2% H2SO4 | Sulphuric Acid | Boiling | 5 |
10% H2SO4 | Sulphuric Acid | Boiling | 12 |
20% H2SO4 | Sulphuric Acid | Boiling | 33 |
50% H2SO4 | Sulphuric Acid | 174 (79) | 16 |
80% H2SO4 | Sulphuric Acid | 199 (93) | 68 |
10% H2SO4 + 1% HCl | Mixed Acid | 194 (90) | 94 |
25% H2SO4 + 200 ppm Cl- | Mixed Acid | 158 (70) | 11 |
23% H2SO4 + 1.2% HCl + 1% FeCl3 + 1% CuCl2 | ASTM G28B | Boiling | 8 |
50% H2SO4 + 42g/l Fe2(SO4)3 | ASTM G28A | Boiling | 40 |
Due to its unparalleled corrosion resistance and high mechanical strength, Alloy 22 is widely utilised in demanding industrial applications, including:
With its proven performance and durability, Alloy 22 is the preferred choice for industries operating under extreme conditions.
Alloy 22 offers a powerful combination of corrosion resistance, mechanical strength, and fabrication flexibility, making it an excellent choice for critical applications across numerous sectors.
Alloy 22 is the ideal material solution for industries requiring proven long-term protection, operational efficiency, and reduced maintenance demands. For further advice or to request a quote, contact our team today.
Can't find the information you need? Please contact us directly.